Relying on mass production and reliable quality, our Liquid Cold Plate with Copper Tube, Cold Forging Heat Sink for LED, Cooling Plate Heat Sinks is well-received in domestic and international markets and has gained a good reputation from our customers. We actively create a warm and harmonious atmosphere to let employees feel the humanistic care of the company and enhance their sense of belonging. We carry out comprehensive staff training, so that employees update their knowledge, broaden their horizons, and improve their skills. We strive to become a trusted partner of our customers, to satisfy them and to speed up the development of the industry.
Brazing
Brazing is the jointing of metals using a molten filler material, which on cooling forms a joint.
The filler metal melting temperature is above 450℃, but below the melting point of the metals.
How does it work?
Brazing joints the base metals by creating a metallurgical bond between the filler metal and the base metals.
When molten, the filler metal is drawn into the joint by capillary action.

How do you supply filler metal to 100's of joint simultaneously?
Brazing sheet!

Aluminum oxide
Aluminum oxide characteristics:
Hardness significantly above 400Mpa
High resistance to chemicals
The oxide interferes with brazing
Aluminum owes many of its properties to very strong adherent oxide film on the surface.
This oxide must be removed or broken up if joining is to occur.
There are a number of possibilities of achieving this.

Comparison of brazing processes:
CAB | Vacuum brazing | Air furnace brazing | |
Heating | Radiation/Convection | Radiation | Forced convection |
Use of flux | Yes | NO | NO |
Quantity of flux | <5g/㎡ | - | 30~50g/m³ |
Pre braze treatment | Moderate demands | High demands | Moderate demands |
Post braze treatment | NO | NO | Yes |
Aqueous wastes | NO | Yes | |
Atmospheric emissions | NO | NO | NO |
Continuos process | Yes | NO | Yes |
Investment | 80 | 100 | 90 |
Operating expense | 80 | 100 | 100 |
CAB furnace brazing process sequence
The CAB process sequence is depending on: Heat exchanger design, Cleaning method, Flux application method.

CAB furnace braze cycle

Factors determining CAB production success or failure
1. Good product fit-up ( gap tolerance 0.1 to 0.15mm)
2. Adequate quantity of filler metal
3. Uniformity of flux coating
4. Interaction of flux and alloying elements
5. Furnace conditions (temperature time profile, temperature uniformity, furnace atmosphere)

Our aim is quality first, the main production Aluminum CNC Machining Water Cooled Plate Heatsink is produced by advanced technology, and has passed the industry certification. We will continue to improve product performance, continue to develop innovative products, and continue to provide users with satisfactory products. The company has been committed to quality and service, and is willing to work hand in hand with our customers to create a better future.
Hot Tags: Vacuum Brazing Process, China, suppliers, manufacturers, factory, customized, free sample, made in China, Round Aluminum Heatsink for LED, Heat Sink, Copper Skived Heat Sink, High Quality Cooling Heat Sink, Aluminum Cold Plates for Battery, Bonded Fin Heat Sinks Assemblies
[[ProKeywords]]